Bitumen 200/300 Specifications

No. Analysis Unit Limit Test Method
1 Density@25 ̊ C Kg/m³ 990-1050 ASTM D70 or D3289
2 Penetration@25 ̊ C Mm/10 200-300 ASTM D5
3 Softening point ̊ C 31 Min. ASTM D36
4 Ductility@25 ̊ C Cm 100 Min. ASTM D113
5 Loss on heating Wt% 1 Max. ASTM D6
6 Drop in penetration after heating % 37 Max. ASTM D5 and D6
7 Flash point ̊ C 177 Min. ASTM D92
8 Solubility in Trichloroethylene Wt% 99.0 Min. ASTM D4
9 Spot test - Negative AASHOT102
10 Viscosity@60 ̊ C P 200+50 ASTM D2171
11 Viscosity@135 ̊ C CST 80 Min. ASTM D2170

 

Usage: The main common usage of bitumen 200/300 is being used in the manufacture of hotmix asphalt for basis and wearing courses road construction.